7.4.4
Problems with RDE
There are various different types of RDE:
GC: Glassy carbon electrode, can be polished with aluminium oxide, glossy
surface.
Au: Gold electrode, can be polished with aluminium oxide, mat surface.
UT: Ultra-trace graphite electrode, can be scraped and polished with alumin-
ium oxide, mat surface.
Ag: Silver electrode, can be polished with aluminium oxide, mat surface.
Pt:
Platinum electrode, looks very similar to Ag, mat surface.
Low background current or unstable base line
•
The electrode surface must be repolished.
•
Has the correct RDE been used?
•
Exchange RDE.
•
Check concentration of electrolyte and pH of the solution.
•
Has the electrode been conditioned (e.g. with
CONDC
) ?
•
Check initial and final potential of the analysis.
•
If the ion concentration in the solution is too high: dilute the electrolyte.
•
If the concentration to be determined is considerably higher than expected:
reduce sample volume.
•
The background current is normally higher if RDE is used in place of MME.
•
A background current of several 100 nA is entirely possible.
•
Electrolyte solution too old: make up a new one. Its working life with organic
additives may be as short as 1 day or less.
Standard addition curves are not reproducible
•
Check program in the instrument (stirring time, etc.).
•
Check RDE (see section 3.5).
•
The pipetting process was not correct: was the pipetting unit used properly?
•
Repeat the analysis again or try out automatic standard addition with Dosi-
mat, Dosino or 6.5611.010 Pipetting equipment.
•
Pipetting the standard solutions must be carried out by one and the same
person or with the same instrument or the same pipette.
•
Check and test pipetting process. When were the pipettes last calibrated
(GLP)?
•
Organic components interfere with the analysis: carry out a UV digestion or
other suitable sample preparation.
•
Are the calibration solutions too old?
•
Would a calibration curve be more suitable?
Peak displacement
•
Check and adjust pH of the solution.
•
Check electrolyte composition and correct if necessary.
•
Organic components interfere with the analysis: carry out a UV digestion or
other suitable sample preparation.