beautypg.com

Aluminum, Air plasma / air shield 130 a cutting, Metric english – Hypertherm HPR260 Manual Gas Preventive Maintenance Program Rev.5 User Manual

Page 128: Marking

background image

OPERATION

4-34

HPR260 Auto Gas

Instruction Manual

4

Aluminum

Air Plasma / Air Shield

130 A Cutting

220198

220173

220181

220176

220179

220197

Note: This process produces a rougher cut edge that is less perpendicular than the 130 A, H35/N

2

process.

Metric

English

Select

Gases

Set

Preflow

Set

Cutflow

Material

Thickness

Arc

Voltage

Torch-to-Work

Distance

Cutting

Speed

Initial Pierce

Height

Pierce Delay

Time

Plasma Shield Plasma Shield Plasma Shield

mm

Volts

mm

mm/m

mm

factor %

seconds

Air

Air

19

31

75

23

6

153

2.8

2370

5.6

200

0.2

10

154

3.0

1465

6.0

0.3

12

156

1225

0.5

15

158

3.3

1050

6.6

0.8

20

162

3.5

725

7.0

1.3

25

172

4.0

525

Edge start

Select

Gases

Set

Preflow

Set

Cutflow

Material

Thickness

Arc

Voltage

Torch-to-Work

Distance

Cutting

Speed

Initial Pierce

Height

Pierce Delay

Time

Plasma Shield Plasma Shield Plasma Shield

in

Volts

in

ipm

in

factor %

seconds

Air

Air

19

31

75

23

1/4

153

0.110

90

0.220

200

0.2

3/8

154

0.120

60

0.240

0.3

1/2

156

45

0.5

5/8

158

0.130

40

0.260

0.8

3/4

162

0.140

30

0.280

1.3

1

172

0.160

20

Edge start

Select

Gases

Set

Preflow

Set

Cutflow

Amperage

Torch-to-Work

Distance

Marking

Speed

Arc

Voltage

Amps

mm

in

mm/min

ipm

Volts

N

2

N

2

10

10

10

10

18

2.5

0.100

6350

250

120

Marking

Flow rates – lpm/scfh

Air

Preflow

73 / 154

Cutflow

78 / 165