Film
Film Selection
For best results, Professional Laminating Systems Inc. recommends using a film that is;
• Manufactured in the USA or name brand and of good quality. This is due to apparent
complexity in the film manufacturing process and the compromise of quality by foreign
manufactures that offers no repercussion to their profits.
• Lower temperature, The lower temperature film used, the longer the rollers will last and the
fewer problems will occur related to excessive heat on the substrate
• Use a film that is at least 75% (3/4) the width of the rollers if narrower film is used one should
make sure that the laminator is run more slowly than usual
• Make sure that the core diameter matches the mandrel size of your machine
• There are a wide range of thickness and types available
Film Type
:
ProLam, inc. recommends using film of good quality from a reputable manufacture. There are many
different variables consistent with all films. Of which the most significant are:
-
Film type - such as polyester, polyethylene, polypropylene, vinyl, nylon and others –
-
Film thickness - such as 1.2, 1.5, 1.8. 2, 3, 5, 7, 10, 15, mils thick -
-
Film to adhesive ratios - just 5 mil alone is available in 4 or more different ratios –
- Different adhesives – this is one of the most important issues when it comes to laminating
especially wide format laminating as there are many different adhesives and many different inks
and papers, an adhesive must be used that is compatible with your ink and media.
- Temperature range - from 160 degrees to 300 degrees never use any laminate rated with a
higher melt point –