Investment material mixing ratio

Investment material

100 g investment ring

200 g investment ring

300 g investment ring

IPS PressveSt

13 ml liquid

9 ml dist. water

26 ml liquid

18 ml dist. water

39 ml liquid

27 ml dist. water

IPS PressveSt Speed

16 ml liquid

11 ml dist. water

32 ml liquid

22 ml dist. water

48 ml liquid

33 ml dist. water

Press parameters

InLine

®

PoM

– Press-on-Metal ceramic

IPS

Press parameters for IPS InLinePoM ingots in the IPS Investment ring System 300 g

Investment Ring
300 g

B

°C/°F

T

°C/°F

H

min

t

°C/°F/min

V

1

°C/°F

V

2

°C/°F

N / E

300 g

EP 500 / V 2.9

700/1292

960/1760

40

60/108

500/932

960/1760

Programm 31–51

eP 600 /

eP 600 combi

700/1292

950/1742

40

60/108

500/932

950/1742

50 µm/min.*

Programat eP 3000 /

Programat eP 5000

700/1292

950/1742

40

60/108

500/932

950/1742

50 µm/min.*

*Important: If you enter the program manually, observe the abort criterion.

Press parameters for IPS InLine PoM ingots in the IPS Investment ring System 100 g and 200 g

Investment Ring
100 g and 200 g

B

°C/°F

T

°C/°F

H

min

t

°C/°F/min

V

1

°C/°F

V

2

°C/°F

N / E

100 g

200 g

EP 500 / V 2.9

700/1292

950/1742

10

20

60/108

500/932

950/1742

0

Program 11-20

eP 600 /

eP 600 combi

700/1292 940/1724

10

20

60/108

500/932

940/1724

250 µm/

min.*

Programat eP 3000 /

Programat eP 5000

700/1292 940/1724

10

20

60/108

500/932

940/1724

250 µm/

min.*