Alloy processing / oxide firing – Ivoclar Vivadent IPS InLine System User Manual

Page 17

background image

17

Metal framework before blasting

Carefully blast the framework with aluminium oxide Al

2

O

3

50–100 µm

(observe the instructions of the alloy manufacturer).

Alloy processing / oxide firing

The cast metal framework is finished using tungsten carbide burs or ceramic-bonded grinding instruments.

After blasting, clean the metal framework with a steam jet and allow to dry thoroughly.
Conduct the oxide firing according to the instructions of the manufacturer.

After oxide firing, the framework should exhibit an evenly oxidized surface.