DURO-LAST

®

40 MIL MEMBRANE

Codes and Standards:

Underwriters Laboratories (US & Canada), FM Approvals, ICC-ES (ESR-1660), State of Florida, Miami-Dade
County, Texas Department of Insurance.

Storage:

Store rolls on their sides and on pallets. Use tarps to keep rolls dry.

Membrane Attachment:

Mechanically Fastened – DL40 membrane may be mechanically attached to a variety of roof deck and wall
materials. An appropriate slip sheet or cover board may be required. Refer to the Duro-Last Mechanically
Fastened Systems Specification for system requirements.

Duro-Bond

®

System – The Duro-Bond system (inductive weld) may be used to attach DL40 membrane. Refer

to the Duro-Last Duro-Bond System Specification for system requirements.

Adhered – DL40 membrane may be adhered to a variety of properly prepared roof decks, walls, cover boards
and insulations including Duro-Guard™ ISO products, DensDeck

®

Prime Roof Board and SECUROCK

®

Gypsum-Fiber Roof Board. Refer to the Duro-Last Adhered Systems Specification for system requirements.

Physical Properties:

DL40 membrane has been subjected to the tests required by ASTM 4434 “Standard Specification for Poly (Vinyl
Chloride) Sheet Roofing”
and has been classified as a Type IV, internally reinforced sheet. The results of each
test are listed below.

Physical Property

Test Method

ASTM 4434 Requirement

Result

Typical Value

Overall Thickness

ASTM D751

≥ 0.036 in.

PASS

40 mil, nominal

Breaking Strength

1

ASTM D751 Grab Method

≥ 275 lbf./in.

PASS

355 lbf x 441 lbf

1

Elongation

1

ASTM D751 Grab Method

≥ 25%

PASS 28%

x

31%

1

Seam Strength

ASTM D 751 Grab Method

≥ 330 lbf

(75% of Breaking Strength)

PASS 360

lbf

Tear Strength

1

ASTM D751 Procedure B

≥ 90 lbf.

PASS

125 lbf x 136 lbf

1

Low Temp. Bend

ASTM D2136

Must Pass at – 40

°F

PASS PASS

Heat Aging

ASTM D3045

Conditioned for 56 days in oven

maintained at 176

°F

PASS PASS

Accelerated Aging

ASTM G154

(formerly G53)

5,000 hour total test time.

Irradiance level of 0.68 W/m2-nm.

Cycle: 8 hour at 145

°F,

4 hour condensation at 122

°F

PASS PASS

Dimensional Stability

1

ASTM D1204

Conditioned for 6 hours in oven

maintained at 176

°F.

Allowable change: ≤ 0.5%

PASS

-0.45% x -0.40%

1

Water Absorption

ASTM D570

Immersed in water at 158

°F

for 168 hours.

Allowable Weight Change: ≤ 3%

PASS 2.6%

Static Puncture

ASTM D5602

≥ 33 lbf

PASS 56

lbf

Dynamic Puncture

ASTM 5635

≥ 14.7 ft-lbf (20 J)

PASS

≥ 14.7 ft-lbf (20 J)

1

Typical values are shown for both machine and cross machine directions. The machine direction results are listed first.

Additional Tests

Fungi Resistance

ASTM G-21

No Sustained growth or discoloration

Moisture Vapor Transmission

ASTM E96, Proc. B, Method A

< 0.22 U.S. Perms