DURO-LAST 50 MIL MEMBRANE

Codes and Standards:

Underwriters Laboratories (US & Canada), FM Approvals, ICC-ES (ESR-1660), Canadian Construction
Materials Centre (CCMC 13299-L), State of Florida, Miami-Dade County, Texas Department of Insurance.

Storage:

Store rolls on their sides and on pallets. Use tarps to keep rolls dry.

Membrane Attachment:

Mechanically Fastened – DL50 membrane may be mechanically attached to a variety of roof deck and wall
materials. An appropriate slip sheet or cover board may be required. Refer to the Duro-Last Mechanically
Fastened Systems Specification for system requirements.

Duro-Bond

®

System – The Duro-Bond system (inductive weld) may be used to attach DL50 membrane. Refer

to the Duro-Last Duro-Bond System Specification for system requirements.

Adhered – DL50 membrane may be adhered to a variety of properly prepared roof decks, walls, cover boards
and insulations including Duro-Guard™ ISO products, DensDeck

®

Prime Roof Board and SECUROCK

®

Gypsum-Fiber Roof Board. Refer to the Duro-Last Adhered Systems Specification for system requirements.

Physical Properties:

DL50 membrane has been subjected to the tests required by ASTM 4434 “Standard Specification for Poly (Vinyl
Chloride) Sheet Roofing”
and has been classified as a Type III, internally reinforced sheet. The results of each
test as well as typical values are listed below.

Physical Property

Test Method

ASTM 4434 Requirement

Result

Typical Value

Overall Thickness

ASTM D751

≥ 0.045 in.

PASS

50 mil, nominal

Breaking Strength

1

ASTM D751 Grab Method

≥ 200 lbf./in.

PASS

390 lbf x 438 lbf

1

Elongation

1

ASTM D751 Grab Method

≥ 15%

PASS

31% x 31%

1

Seam Strength

ASTM D 751 Grab Method

≥ 292 lbf x 328 lbf

(75% of Breaking Strength)

PASS 417

lbf

Tear Strength

1

ASTM D751 Procedure B

≥ 45 lbf.

PASS

132 lbf x 163 lbf

1

Low Temp. Bend

ASTM D2136

Must Pass at – 40

°F

PASS PASS

Heat Aging

ASTM D3045

Conditioned for 56 days in oven

maintained at 176

°F

PASS PASS

Accelerated Aging

ASTM G154

(formerly G53)

5,000 hour total test time.

Irradiance level of 0.68 W/m2-nm.

Cycle: 8 hour at 145

°F,

4 hour condensation at 122

°F

PASS PASS

Dimensional Stability

1

ASTM D1204

Conditioned for 6 hours in oven

maintained at 176

°F.

Allowable change: ≤ 0.5%

PASS

-0.30% x -0.45%

1

Water Absorption

ASTM D570

Immersed in water at 158

°F

for 168 hours.

Allowable Weight Change: ≤ 3%

PASS 1.7%

Static Puncture

ASTM D5602

≥ 33 lbf

PASS 56

lbf

Dynamic Puncture

ASTM 5635

≥ 14.7 ft-lbf (20 J)

PASS

≥ 14.7 ft-lbf

1

Typical values are shown for both machine and cross machine directions. The machine direction results are listed first.

Additional Tests

Fungi Resistance

ASTM G-21

No Sustained growth or discoloration

Moisture Vapor Transmission

ASTM E96, Proc. B, Method A

< 0.22 U.S. Perms