Codes and Standards:
Underwriters Laboratories (R10128).
Storage:
Store rolls on pallets. Use tarps to keep rolls dry.
Membrane Attachment:
Adhered – DF60 membrane may be adhered to a variety of properly prepared roof decks, walls, cover boards
and insulations including structural concrete, gypsum, lightweight concrete, DensDeck
®
Prime Roof Board,
SECUROCK
®
Gypsum-Fiber Roof Board, and Duro-Guard
®
ISO products. It may be adhered directly to an
existing built-up roof (BUR) by using Duro-Fleece
®
Adhesive or splatter applied Duro-Grip
®
CR-20. Prior written
approval from the Duro-Last Engineering Services Department is required prior to adhering to BUR. Refer to the
Adhered Duro-Fleece Roofing System Specification for substrate preparation and acceptable adhesives.
Mechanically Fastened – DF60 membrane may be mechanically attached to a variety of roof deck and wall
materials. An appropriate slip sheet or cover board may be required. Refer to the Duro-Last Mechanically
Fastened Systems Specification for system requirements.
Physical Properties:
DF60 membrane has been subjected to the tests required by ASTM 4434 “Standard Specification for Poly (Vinyl
Chloride) Sheet Roofing” and has been classified as a Type III, internally reinforced sheet with a fabric backing.
The results of each test as well as typical values are listed below.
Physical Property
Test Method
ASTM 4434 Requirement
Result
Typical Value
Overall Thickness
ASTM D751
0.045 in.
PASS
60 mil, nominal
(with fleece: 78 mil)
Thickness Over Scrim
ASTM D7635
0.016 in.
PASS 32
mil
Breaking Strength
1
ASTM D751 Grab Method
200 lbf./in.
PASS
554 lbf x 408 lbf
1
Elongation
1
ASTM D751 Grab Method
15%
PASS 34%
x
85%
1
Seam Strength
ASTM D 751 Grab Method
306 lbf.
(75% of Breaking Strength)
PASS 322
lbf
Tear Strength
1
ASTM D751 Procedure B
45 lbf
PASS
50 lbf x 200 lbf
1
Low Temp. Bend
ASTM D2136
Must Pass at – 40
F
PASS PASS
Heat Aging
ASTM D3045
Conditioned for 56 days in oven
maintained at 176
F
PASS PASS
Accelerated Weathering
ASTM G154
(formerly G53)
5,000 hour total test time.
Irradiance level of 0.68 W/m2-nm.
Cycle: 8 hour at 145
F,
4 hour condensation at 122
F
PASS PASS
Dimensional Stability
1
ASTM D1204
Conditioned for 6 hours in oven
maintained at 176
F.
Allowable change: ≤ 0.5%
PASS 0.11%
x
0.00%
1
Water Absorption
ASTM D570
Immersed in water at 158
F
for 168 hours.
Allowable Weight Change: ≤ 3%
PASS 2.4%
Static Puncture
ASTM D5602
33 lbf
PASS
33 lbf
Dynamic Puncture
ASTM 5635
14.7 ft-lbf (20 J)
PASS
14.7 ft-lbf
1