23

Condition the surface using e.g. Telio Activator.

Roughening, SR Connect

Apply Telio Lab.

Apply SR Nexco.

b) Use of SR Connect

Apply a thin layer of SR Connect on the conditioned surface of the area to be supplemented using a disposable brush,
allow to react for 2–3 min and subsequently polymerize. Then, layer Telio Lab LC or SR Nexco materials (see Telio CAD/Lab
or SR Nexco Instructions for Use).

With Telio Lab (cold-curing):

Blast the area to be supplemented (Al

2

O

3

, 100 µm, 1-2 bar / 15-29 psi). Then clean with steam and dry with oil-free com-

pressed air. Subsequently, condition with Telio Activator or Telio Lab Cold Liquid. For this purpose, distribute Telio Activator
evenly but generously on the conditioned surface and allow it to react for at least 2 min to a maximum of 4 min. Then
directly begin with the application of the Telio Lab material (see Telio CAD/Lab Instructions for Use).

After polymerization finish with cross-cut tungsten carbide burs and prepolish with rubber polishers and silicone wheels. A