4.06 Cut Quality

Cut quality requirements differ depending on application. For instance, nitride build-up and bevel angle may be
major factors when the surface will be welded after cutting. Dross-free cutting is important when fi nish cut quality
is desired to avoid a secondary cleaning operation. Cut quality will vary on different materials and thicknesses.

Right Side

Cut Angle

Left Side

Cut Angle

A-00512

Kerf Width

Cut Surface
Bevel Angle

Top Edge

Rounding

Cut Surface

Drag Lines

Dross

Build-Up

Top

Spatter

A-00007

Cut Surface

The condition (smooth or rough) of the face of the cut.

Bevel Angle

4. Place the RUN/SET switch to the RUN position.

The angle between the surface of the cut edge and a plane perpendicular to the surface of the plate. A perfectly
perpendicular cut would result in a 0° bevel angle.

Top-Edge Rounding

Rounding on the top edge of a cut due to wearing from the initial contact of the plasma arc on the workpiece.

Dross Build-up and Top Spatter

Dross is molten material which is not blown out of the cut area and re-solidifi es on the plate. Top spatter is
dross which accumulates on the top surface of the workpiece. Excessive dross may require secondary clean-up
operations after cutting.

Kerf Width

The width of material removed during the cut.

Nitride Build-up

Nitride deposits which may remain on the cut edge of the carbon steel when nitrogen is present in the plasma
gas stream. Nitride buildups may create diffi culties if the steel is welded after the cutting process.