GC EUROPE Fujivest Super User Manual
Page 21

21
Focus Edition from GC
Perfectly cast objects
Heating-up schedules
>
>
3.2.2 Process of a Step- Heating schedule (Conventional technique)
SLH
The investment material is allowed to set for 20 min and then placed in the burnout furnace at room
temperature; it is then heated up in a series of temperature steps, before being heat soaked at the final
end temperature for a period as indicated in the ‘Instructions for Use’ prior to being cast.
High temperatures assuring a complete burnout
of all pattern materials, extra stimulated by a
“steam” effect