wet the areas to be bonded to extraorally with Telio
Activator. Brush Telio Activator into the entire surface for at
least 30 seconds using an application brush in order to
ensure an even distribution and quick penetration of Telio
Activator. Subsequently, allow the Activator to react for
another 30–60 seconds (total reaction time 1-2 minutes).
Now apply the Heliobond bonding agent, thinly disperse it
with blown air and polymerize for 10 seconds (650 mW/cm
2
,
e.g. bluephase
®
using LOP).
Apply Telio CS C&B directly to the conditioned surface for
the relining.
Please refer to the corresponding Instructions for Use (Telio
Chairside or Telio Labside) for the detailed working steps
regarding the relining with Telio CS C&B.
• Subsequent addition of material / repairs of Telio CS
C&B restorations with Telio Add-On Flow
Roughen the area to be supplemented or repaired using
coarse diamonds or sandblast (Al
2
O
3
, 100 µm, 1–2 bar/
15–29 psi). Thoroughly rinse with water and dry with oil-free
compressed air. Then wet the areas to be bonded to extra-
orally with Telio Activator. Brush Telio Activator into the
entire surface for at least 30 seconds using an application
brush in order to ensure an even distribution and quick
penetration of Telio Activator. Subsequently, allow the
Activator to react for another 30-60 seconds (total reaction
time 1-2 minutes). Now apply the Heliobond bonding agent,
thinly disperse it with blown air and polymerize for
10 seconds (650 mW/cm
2
, e.g. bluephase using LOP).
Apply Telio Add-On Flow or a light-curing Ivoclar Vivadent
composite (e.g. Tetric EvoFlow, Tetric EvoCeram) and cure
according to the Instructions for Use.
Application in the dental laboratory
• Customization of / addition of material to Telio CAD /
Telio Lab restorations using
– Telio Lab
– Telio Stains
– Telio Lab LC Massen
– Telio Add-On Flow
Roughen the area to be supplemented by grinding or sand-
blast (Al
2
O
3
, 100 µm, 1–2 bar/15–29 psi). Then thoroughly
clean with steam and dry with oil-free compressed air. After
that, condition with Telio Activator. For that purpose,
distribute Telio Activator evenly and generously on the
conditioned surface and allow it to react for at least
2 minutes to a maximum of 4 minutes.
After the reaction time has passed, Telio Lab can be directly
applied. If the other materials mentioned are used (Telio
Stains, Telio Lab LC materials and Telio Add-On Flow), apply
SR Composiv to the activated surfaces according to the
Instructions for Use in a first step and then polymerize.
Subsequently, the Telio Stains, Telio Lab LC materials are
layered to customize the restoration.
Please refer to the corresponding Instructions for Use (Telio
Lab/CAD) for the detailed working steps regarding the
individualization or add-ons.
Overview of material combinations and processing
Warning
– Telio Activator contains methyl methacrylate (MMA).
– MMA is highly flammable and irritating (flash point:
+10 °C/50 °F).
– Do not inhale vapours.
– Irritating to eyes, respiratory organs and skin
– Skin contact may cause sensitization. Customary medical
Restorative
Surface
1
) Surface
Add-on
material
Preparation
Activation
material
2
) Bonding
Agent
Telio CS C&B
Blasting (Al
2
O
3
,
100 µm, 1–2 bar/
15-29 psi pressure),
or roughening with
a coarse diamond
1
) Telio Activator
2
) Heliobond
Telio CS C&B
Telio Add-On
Flow
Telio Stains
Telio Lab /
Telio CAD
Blasting (Al
2
O
3
,
100 µm, 1–2 bar/
15-29 psi pressure),
or roughening
with rotary
instruments
1
) Telio Activator
2
) Heliobond
Telio CS C&B
Telio Add-On
Flow
Telio Stains
Ivoclar Vivadent
denture teeth
made of PMMA
and composite
(excluding
ceramic teeth )
Blasting (Al
2
O
3
,
100 µm, 1–2 bar/
15-29 psi pressure),
or roughening
with rotary
instruments
1
) Telio Activator
or
1
) Telio Lab Cold
Liquid
Telio Lab
1
) Telio Activator
or
1) Telio Lab Cold
Liquid
Telio Lab
1
) Telio Activator
or
1
) Telio Lab Cold
Liquid
2
) SR Composiv
Telio Stains
Telio Lab LC
Telio Add-On
Flow