Finish the temporary restoration with rotary instruments (cross-cut tungsten carbide burs).
Use diamond disks to finish the interdental areas.
Polishing with silicon carbide rubber polishers (e.g. OptraPol).
Polishing with a cotton buffing wheel
Curing and finishing
After removing the temporary restoration from the impression (or from the tooth preparation), remove
excess material using rotary instruments once the material is cured completely (after approx. 4 to
5 minutes). Cross-cut tungsten carbide burs are suitable for finishing. Remove the inhibition layer with
alcohol or by polishing. Silicon carbide rubber polishers (e.g. OptraPol) should be used for polishing.