Firing parameters for glaze firing with glazing material

T

830°C

1526°F

B

403°C

757°F

S

4 min.
4 min.

t

60°C

108°F

H

1–2 min.
1–2 min.

V

1

450°C

842°F

V

2

829°C

1524°F

Important

If furnaces of other manufacturers are used, these

parameters have to be adjusted accordingly.

Avoid pooling and the application of too thick layers.

Apply glazing material in the usual manner using a brush.

Method 2

Glaze firing with glazing material
Remove IPS d.SIGN Glazing material from it’s container and
mix thoroughly. If another consistency is desired, the material
can be slightly diluted with IPS d.SIGN Glazing and Staining
liquid. After that, apply glazing material in the usual manner
using a brush. Avoid pooling and the application of too thick
layers. If desired, make minor shade adjustments on the
applied glazing material using IPS d.SIGN Shade, Stains, and
Essence.

Completed IPS d.SIGN restorations

Apply minor shade adjustments on the applied
glazing material using IPS d.SIGN Shade, Stains, and
Essence.