Ivoclar Vivadent IPS d.SIGN User Manual
Page 35

35
Firing parameters for the 1
st
shoulder firing
T
890°C
1634°F
B
403°C
757°F
S
6 min.
6 min.
t
60°C
108°F
H
1 min. 
1 min. 
V
1
450°C
842°F
V
2
889°C
1632°F
➚
Important
If furnaces from other manufacturers are used,
these parameters have to be adjusted accordingly.
Apply IPS d.SIGN Margin material generously in the cervical area in the shape of a drop…
... and dry.
Carefully remove the framework with the applied and dried shoulder material from the die.
Fire the restoration using the firing parameters for the 1
st
shoulder firing.
Sinter shrinkage of the shoulder after the 1
st
shoulder firing.
Tip:
When designing a ceramic shoulder (particularly for
bridges), the Margin material may be applied higher up in
the proximal areas. This will reduce interdental shrinkage
during the subsequent dentin and incisal firings.
- 14K (2 pages)
 - 24K (2 pages)
 - BioUniversal KFG (2 pages)
 - Capricorn 15 (2 pages)
 - Callisto 86 (2 pages)
 - Harmony KF (2 pages)
 - Callisto 86 (2 pages)
 - BioUniversal KFG (2 pages)
 - BioUniversal KFG (2 pages)
 - BioUniversal E (2 pages)
 - BioUniversal PdF (2 pages)
 - Brite Gold (2 pages)
 - Capricorn 15 (2 pages)
 - Callisto Implant 33 (2 pages)
 - Capricorn (2 pages)
 - Colado CC (2 pages)
 - Callisto 84 (2 pages)
 - Callisto CP+ (2 pages)
 - Callisto CPG (2 pages)
 - Callisto Implant 60 (2 pages)
 - CosmoPost (24 pages)
 - Colado NC (2 pages)
 - Elektra (2 pages)
 - Evolution Lite (2 pages)
 - ESPRIT (1 page)
 - Elektra 10 (2 pages)
 - IPS d.SIGN Ultra (2 pages)
 - EP 5000 (1 page)
 - Harmony 2 (2 pages)
 - EP 600 (36 pages)
 - Harmony Hard (2 pages)
 - Harmony Medium (2 pages)
 - Harmony Soft (2 pages)
 - Heliobond (36 pages)
 - Harmony 3 (2 pages)
 - Harmony C&B 55 (2 pages)
 - EP 600 Combi (40 pages)
 - Harmony PF (2 pages)
 - Harmony X-Hard (2 pages)
 - IPS AcrylCAD (2 pages)
 - IPS d.SIGN 30 (2 pages)
 - IPS Classic (24 pages)
 - IPS d.SIGN 59 (2 pages)
 - IPS d.SIGN 84 (2 pages)
 - IPS d.SIGN 96 (2 pages)
 