AWAPLAN
TM
APPLICATION INSTRUCTIONS
BASE PLY
Install one or more base plies prior to the application of AWAPLAN. TAMKO Glass-Base
®
, Type 43 Organic Base
Sheet, Tam-Ply IV
®
, and Versa-Base
®
are the recommended base ply materials. Alternatively, base sheets that meet the
requirements of ASTM D4601, Type II; ASTM D2178, Type IV or Type VI; ASTM D2626; ASTM D6163, ASTM D6164
or ASTM D4897, Type II are acceptable. The base sheet shall have minimum side laps of 2 in. and end laps of 4 in.
Not all application methods apply to all base sheets. Certain base plies are limited in the manner in which they may be
applied. Consult the base ply manufacturer’s application instructions for the base ply used and the current National Roofing
Contractor Association (NRCA) Manual - Membrane Roof Systems for installation instructions. See the chart below for
information regarding acceptable application methods of TAMKO base sheets.
HOT ASPHALT APPLICATION
Interply moppings of asphalt shall consist of approximately 23 lbs. (±15%) per 100 sq. ft. of roof area. For any surfaces
including insulating materials which absorb asphalt, it may be necessary to apply the asphalt in greater quantities to assure
adequate adhesion. Avoid excessive interply moppings as slippage may result. The asphalt must meet ASTM D312,
Type III for slopes up to ¼ in. and Type IV for slopes up to 3 in. The asphalt must be a minimum of 400°F at the point of
application. MOP NO FURTHER THAN 4 FT. IN FRONT OF THE ROLL. Immediately press the roll into the hot asphalt
by applying pressure to the factory core in the roll. The AWAPLAN membrane shall have side laps of 4 in. and end laps
of 6 in. The entire sheet, including the side and end laps, must be totally adhered in asphalt with no void areas. A small
amount of asphalt protruding from the side and end laps is acceptable. However, care should be taken to avoid excessive
amounts of asphalt at the lap. All exposed asphalt in excess of ¼ in. width should be covered with granules.
COLD ADHESIVE APPLICATION
TAM-PRO® M3 Adhesive or TAM-PRO 856 Premium SBS Adhesive may be applied using a 3/16” V notched squeegee
or TAM-PRO M3 Adhesive may be applied using spray equipment designed for this purpose. The rate of application is
approximately 1-1/2 gallons per square for squeegee application and 1-1/2 to 2-1/2 gallons per square for spray application.
CAUTION: Using excessive amounts of cold adhesive may cause blistering or damage to the finished AWAPLAN
membrane.
For TAM-PRO 856 Premium SBS Adhesive, the side and end laps must be set in adhesive or heat welded.
For TAM-PRO M3 Adhesive, it is recommended that the side and end laps be heat welded.
Use same technique as outlined in HOT ASPHALT APPLICATION for side and end laps. Use adhesive only in well-
ventilated areas.
Alternatively, a cold process adhesive that meets the requirements of ASTM D3019, Type III may be used. Follow the
manufacturer’s application requirements.
Application Method
Product Name
Hot Asphalt
Mechanically Fastened
Cold Process Adhesive
TAMKO Glass-Base
®
Yes
Yes
No
Tam-Ply IV
®
Yes
No
No
Type 43 Coated Organic Base
Yes
Yes
No
Versa-Base
®
Yes
Yes
Yes