Spray Gun Troubleshooting

DEFECTS

CAUSE

CORRECTION

Coarse spray

Low pressure

Increase the pressure

Excessive fogging

High pressure

Reduce pressure for satisfactory pattern

(overspray)

Material too thin

Use less thinner

Pattern too wide

Spray angle too large

Use smaller spray angle tip

Pattern too narrow

Spray angle too small

Use larger spray angle tip. (If coverage is OK,

try tip in same nozzle group)

Too much material

Tip size too large

Use next smaller tip

Material too thin

Pressure too high

Reduce pressure

Too little material

Tip size too small

Use next larger tip

Material too thick

Thin distribution in

Worn tip

Change for new tip

center of pattern

Wrong tip

Use tip with a smaller spray angle

"horns"

Thick skin on work

Material too viscous

Thin material

Application too heavy

Reduce pressure and/or use smaller tip

Coating fails to

Material too viscous

Thin material

close & smooth over

Spray pattern irregular,

Orifice clogged

Clean carefully

deflected

Tip damaged

Replace with new tip

Craters or pock marks

Solvent balance

Use 1-3% "short" solvents remainder "long"

solvents. (This is most likely to happen with

material of low viscosity, lacquers etc.)

Bubbles on work

Contamination or dust

Clean surface to be sprayed

Clogged screens

Extraneous material

Clean screen

in paint.

Coarse pigments

Use coarse screen if orifice size allows

Poorly milled pigments

Use coarser screen, larger orifice tips. Obain ball

(paint pigments glocculate

milled paint. If thinner was added, test to see if a

cover screen. Incompatible

drop on top of

paint mixes or flattens out on

paint mixture & thinners.

on the surface. If not, try different thinner

in fresh batch of paint.

TEST THE PATTERN