WIRE FEED SPEED CONTROL:
This control sets the feed speed of the wire feeder. Turn the knob to the left for slower speeds and to
the right for higher speeds. The control is calibrated. The nameplate shows the wire speed for the given
setting of the control.
Controls the direction the wire is being fed thru the feeder.
Up to return wire to the spool. Down to feed
the wire to the gun in order to weld.
The manual position allows the operator to rotate the machine without welding to check the wire
placement as well as the cam setting. The auto side will start the entire weld operation based on the
operators settings, including machine rotation.
PREFLOW CONTROL:
This control, provides flow of shielding gas to the work before the arc is established. The gas solenoid
valve is energized immediately when the gun trigger is closed, but the time delay before the wire feeder
is energized is adjustable from 0 to 1.5 seconds. Turn the knob to the left for shorter delays and to the
right for longer delays.
POSTFLOW CONTROL:
This control provides flow of shielding gas to the work after welding has stopped. Delay for the gas
solenoid valve shutoff is adjustable from .5 to 4.5 seconds. Turn the knob to the left for shorter delays and
to the right for longer delays.
PURGE - UP / COLD INCH - DOWN SWITCH:
This control provides control of some wire feeder functions without energizing the welding power source.
The momentary up position energizes the gas solenoid but not the wire feeder or welding power source. The
momentary down position energizes the wire feeder but not the gas solenoid or the welding power source.
BURNBACK CONTROL:
WIRE FEED SPEED
WIRE DIRECTION
PREFLOW
PURGE - UP
COLD INCH - DOWN
MANUAL / AUTO
POSTFLOW
BURNBACK
This control provides a precise time delay that allows the wire to be burned off at the end of the weld.
This is useful for those applications where higher speed, fine wire feeding is used and there is a tendency
for the electrode to overrun at the end of the weld and cause “sticking” in the crater. The delay is
adjustable for optimum burnback depending on wire size, process, procedure, etc.
WIRE DIRECTION:
MANUAL/AUTO:
CWO-3332 WIRE FEEDER CONTROLS